Coating Material Type | HVOF Coatings | Wire Spray Coatings | Plasma Spray Coatings |
PTA Cladding |
Stainless Steel (HRc 25 – 35) |
SS 316, 316L, 420, 174 PH |
SS 316, 316L, 420, 174 PH |
SS 316, 316L, 420, 174 PH |
SS 316, 316L, 420, 174 PH |
Carbon Steels (HRc 25 – 45) |
0.2 – 0.8C, Fe CrAly, FeCrB |
0.2-0.8 C Steels | 0.2 – 0.8C, Fe CrAly | Fe Cr B |
Non Ferrous Alloys |
AI Bronze, Ph Bronze |
Al, Cu, Zn, Bronzes, Babbitt |
Al, Cu, Zn, Bronzes Babbitt |
– |
Ni Alloys (HRc 25-60) |
Ni Al, NiCr, NiCrB alloys Inconels, Hastealloys 625, 718, C276, C22, etc. |
Ni Al, NiCr, NiCrB alloys Inconels, Hastelloys 625, 718 |
Ni, Al, NiCr, NiCrMo alloys Inconels, Hastelloys 625, 718, C276, C22, etc. |
NiCr, NiCrBFe Inconels, Hastelloys 625, 718, C276, C22, etc. |
Cobalt alloys (HRc 38-52) |
Stellite 1, 12, 6 | – | Stellite 1, 12, 6 | Stellite 1, 12, 6, F |
Moly alloys (HRc 40-55) |
Mo, Mo+SF, Mo+oxide | Pur Mo | Mo, Mo+SF, Mo+oxide | – |
Carbides (HV 900-1400) |
Wc/Co: 93/7, 88/12, 8317, WC Co CR, WcCrCNi CrC, Crc+NiCr |
– | WC/Co: 93/7, 88/12, 8317, WC Co CR, WcCrCNi CrC, CrC+NiCr |
WC + SF Alloy |
Oxides
|
Al. Oxide, Al+Ti Oxide, Cr Oxide, ZrO2+8%*5Yt (TBC) |
– | Al. Oxide, Al+Ti Oxide, Cr Oxide, ZrO2+8%*5Yt (TBC) |
– |
polymers / Teflon
|
Anti stick coating over HVOF coating |
Anti stick coating over wire coating |
Anti stick coating over plasma coating |
– |
Specials | Hard Chrome replacement, Carbide + Teflon Blend |
Heavy build up | Special ceramics and oxides |
Heavy abrasion resistant deposits for mud appl. |
Process Features | HVOF | Wire Spray | Plasma Spray | PTA Cladding |
Bond strength | >10000 PSI | ~ 3000 PSI | ~ 8000 PSI | Metallurgical |
Density | ~99% | ~90-95% | ~95-98% | 100% |
Thickness | Metal alloys ~1.5 | Ferrous ~2mm | Metal alloys ~1 | No Limit |
Capability | mm Carbides ~1mm | Non ferrous | ~5mm Mm Carbides and oxides ~0.8 |
– |
Tem. Resistance of coatings |
Medium | Medium | Extremely High (oxide ceramics) |
Good (Satellites) |
Wear resistance of coatings |
Medium | Medium | Good | High |
Heat input to job | Neglible (<150c) | Neglible (<150c) | Neglible (<150c) | High (> 800 C) |
NOTE: Values and features mentioned are indicative of each process and material class, please ask for detailed individual process and coating characteristics.